National grade and coil specifications for carbon steel mild steel aluminized and stainless tube feedstock
Technical procurement and manufacturing reference | 17 November 2026 | Units: mm, MPa, mass % unless stated otherwise
Purpose and interpretation
This guide connects raw-material/coil designations with specifications for finished tubes. A grade alone does not define a compliant tube: the purchase order must also identify product form, applicable edition, dimensions, tolerance class, delivery condition, testing, inspection and documentation. Tables are curated commercial grade families, not a reproduction of copyrighted standards or an assertion that every grade ever standardized is included.
Important conformity principle
A comparison such as ASTM 304 ≈ EN 1.4301 ≈ a GOST chromium–nickel grade is a screening aid only. Chemical limits, deoxidation, stabilization, mechanical requirements, permitted processes, heat treatment and tests can differ. Never print an untested alternative standard on an MTC, and never treat a flat-sheet standard as finished-tube certification.
Chinese national steel material standards
| Norm | Title and product scope | Relevance to Dumai |
|---|---|---|
| GB/T 700 | Carbon structural steels | Q195/Q215/Q235/Q275 family; structure feedstock |
| GB/T 699-2015 | Quality carbon structural steels | 08, 10, 15, 20, 35, 45; chemistry-based engineering grades |
| GB/T 1591 | High-strength low-alloy structural steels | Q355 and related grades; edition and thickness dependent |
| GB/T 5213-2019 | Cold-rolled low-carbon sheet and strip | DC01, DC03, DC04, DC05, DC06 forming family |
| GB/T 13237-2026 | Cold-rolled quality carbon steel sheet and strip | Check effective date and applicability for coil orders |
| GB/T 36399-2018 | Continuously hot-dip Al–Si coated steel sheet/strip | Critical standard for DX grades with AS coating |
| GB/T 2518-2019 | Continuously hot-dip zinc and zinc-alloy coated sheet | NOT the same as AS aluminium–silicon coating |
| GB/T 20878-2024 | Stainless steel designations and chemistry | Current national stainless grade naming/chemistry |
| GB/T 3280-2015 | Cold-rolled stainless flat products | 300/400 stainless cold-rolled tube feedstock |
| GB/T 4237 | Hot-rolled stainless flat products | Hot-rolled substrate, grade and delivery conditions |
| GB/T 222 | Chemical analysis permissible variations | Product analysis tolerance framework |
| GB/T 228.1 | Metallic tensile test at room temperature | Tensile/yield/elongation testing |
Chinese carbon steel and cold forming grades
| Grade | National norm | Mechanical or grade meaning | Tube forming relevance |
|---|---|---|---|
| Q195 | GB/T 700 | Nominal yield classification around 195 MPa | General forming / welded mechanical tube feedstock |
| Q215 | GB/T 700 | Nominal yield classification around 215 MPa | Structural applications by quality class |
| Q235A/B/C/D | GB/T 700 | Nominal yield minimum ~235 MPa for thinner sections | Quality and impact-testing variants |
| Q275 | GB/T 700 | Nominal yield classification around 275 MPa | Higher strength, formability qualification |
| 08/08Al | GB/T 699 / GB/T 5213 product-dependent | Very low-carbon grades | Soft forming and ERW |
| 10/15/20 | GB/T 699 | Quality carbon steel, approx 0.10/0.15/0.20 C name | Check heat analysis, deoxidation and condition |
| 35/45 | GB/T 699 | Medium carbon | Higher strength with more difficult welding |
| Q355 | GB/T 1591 | HSLA structural steel | Do not substitute for Q235 without process/design review |
| DC01/DC03 | GB/T 5213-2019 | Cold-rolled commercial/drawing | Correspondence to EN same names only after edition tests |
| DC04/DC05/DC06 | GB/T 5213-2019 | Deep/extra-deep drawing | Low yield, aging, r- and n-value matter |
Cold rolled DC grades in Chinese GB/T 5213
GB/T 5213-2019 includes DC grades familiar from EN purchasing. For Chinese certification state GB/T 5213-2019 rather than merely DC01 or an assumed EN equivalence. Confirm product thickness, orientation, chemical maxima, yield and tensile values, elongation, r/n forming measures, surface quality and aging conditions on the actual mill certificate. Different national editions can specify different test conditions.
Chinese aluminum–silicon coated steel
| Grade or coating | Technical meaning | Purchase verification |
|---|---|---|
| DX51D+AS | Commercial formable substrate | Coil grade under GB/T 36399-2018 |
| DX52D+AS | Drawing substrate | Confirm availability and GB grade designation |
| DX53D+AS | Deep drawing substrate | Standard designation example explicitly uses DX53D+AS |
| DX54D+AS | Severe forming quality | Relevant to Dumai DX54D+AS120 supply |
| DX55D+AS | High formability | Check listed edition and mechanical performance |
| DX56D+AS | Enhanced drawing | Higher formability; welding must be qualified |
| AS80 | 80 g/m² total nominal coating class | Confirm test method and min spot values |
| AS120 | 120 g/m² total nominal coating class | Coating mass ≠ precise coating thickness |
| AS150 | 150 g/m² total nominal coating class | Check availability, bend cracking and weld seam |
The correct coating standard
GB/T 36399-2018 is the direct Chinese continuously hot-dip aluminium–silicon coated sheet and strip norm, applicable to the DX forming substrates with +AS. GB/T 2518-2019 covers Zn and Zn-alloy coatings and cannot be substituted for +AS. The Chinese standards committee also has a 2026 revision project combining metallic-coating standards, but a project is not itself an effective replacement of GB/T 36399-2018.
Coating verification
Request the exact Chinese standard/edition, steel substrate grade, coating code, minimum total coating mass, spot test convention, bend adhesion results, surface treatment, coil width/thickness, and process tolerances. Record whether the measured tube wall comprises base metal only; coating mass quoted for coil cannot certify finished-tube OD, weld seam corrosion or bend resistance.
Chinese stainless grades and cross-reference register
| Chinese steel name | International screening name | Family | Key chemistry |
|---|---|---|---|
| 06Cr19Ni10 | 304 / UNS S30400 | austenitic | Cr ~18–20; Ni ~8–11; C ≤0.08 (screening) |
| 022Cr19Ni10 | 304L / UNS S30403 | austenitic low carbon | Cr ~18–20; Ni ~8–12; C ≤0.03 (screening) |
| 06Cr17Ni12Mo2 | 316 / UNS S31600 | austenitic molybdenum | Cr ~16–18; Ni ~10–14; Mo ~2–3 |
| 022Cr17Ni12Mo2 | 316L / UNS S31603 | austenitic low-C molybdenum | Mo ~2–3; C ≤0.03 |
| 06Cr18Ni11Ti | 321 / UNS S32100 | austenitic Ti stabilized | Cr ~17–19; Ni ~9–12; Ti stabilization |
| 06Cr18Ni11Nb | 347 / UNS S34700 | austenitic Nb stabilized | Nb stabilization; heat analysis essential |
| 015Cr21Ni26Mo5Cu2 | 904L / UNS N08904 broad analogue | high alloy austenitic | Cr/Ni/Mo/Cu high alloy; verify exact CN chemistry |
| 022Cr11Ti | 409L family | ferritic stabilized exhaust | Cr ~10.5–12.5; Ti; C low |
| 06Cr13Al | 405 family | Al-alloyed ferritic stainless | Cr ~11.5–14.5; Al alloying; NOT aluminized coating |
| 06Cr17 | 430 family | ferritic chromium | Cr ~16–18 |
| 022Cr18Ti | 439 family | Ti-stabilized ferritic | Cr ~17–19; controlled Ti |
| 019Cr19Mo2NbTi | 444 family / comparison only | Mo–Nb–Ti ferritic | Cr ~18–20; Mo ~2; Ti+Nb |
| 019Cr19NbTi | 441-type comparison; confirm grade listing | Nb–Ti ferritic | Specific chemistry/order certification |
China GB/T 20878-2024 governs national stainless steel designation and chemistry. Similar AISI/EN names in the table provide cross-search only; no cross-certification should be declared without simultaneously meeting the entire applicable foreign standard. Chinese stainless flat-product mechanical and surface requirements come from GB/T 3280-2015 or the appropriate hot-rolled flat norm.
300 series stainless grade register
| AISI / trade | UNS | EN screening cross-reference | Main tube relevance | Indicative chemistry, not acceptance limits |
|---|---|---|---|---|
| 301 | S30100 | 1.4310 X10CrNi18-8 | austenitic; high work hardening; formed parts | Cr 16–18; Ni 6–8; C ≤0.15 |
| 302 | S30200 | 1.4319 (comparison only) | austenitic; higher C than 304 | Cr 17–19; Ni 8–10; C ≤0.15 |
| 303 | S30300 | 1.4305 X8CrNiS18-9 | free-machining; sulfur; poor welding choice | Cr 17–19; Ni 8–10; S ≥0.15 |
| 304 | S30400 | 1.4301 X5CrNi18-10 | general welded tube and fabrication | Cr 18–20; Ni 8–10.5; C ≤0.08 |
| 304L | S30403 | 1.4307 / 1.4306 | lower carbon; welded assemblies | Cr 18–20; Ni 8–12; C ≤0.03 |
| 304H | S30409 | 1.4948 (check product) | elevated temperature; controlled carbon | C 0.04–0.10; Cr 18–20; Ni 8–11 |
| 305 | S30500 | 1.4303 X4CrNi18-12 | deep forming; higher nickel | Cr 17–19; Ni 11–13 |
| 309S | S30908 | 1.4833 X12CrNi23-13 | heat oxidation service | Cr 22–24; Ni 12–15; C ≤0.08 |
| 310S | S31008 | 1.4845 X8CrNi25-21 | heat-resistant high chromium nickel | Cr 24–26; Ni 19–22; C ≤0.08 |
| 316 | S31600 | 1.4401 X5CrNiMo17-12-2 | molybdenum for chloride resistance | Cr 16–18; Ni 10–14; Mo 2–3 |
| 316L | S31603 | 1.4404 / 1.4432 / 1.4435 | welded chemical and hygienic tubes | C ≤0.03; Cr 16–18; Mo 2–3 |
| 316Ti | S31635 | 1.4571 X6CrNiMoTi17-12-2 | Ti stabilized; hot service | Cr 16.5–18.5; Ni 10.5–13.5; Mo 2–2.5 |
| 317L | S31703 | 1.4438 (comparison only) | higher Mo; aggressive service | Cr 18–20; Ni 11–15; Mo 3–4 |
| 321 | S32100 | 1.4541 X6CrNiTi18-10 | Ti stabilized exhaust and heat | Cr 17–19; Ni 9–12; Ti controlled |
| 347 | S34700 | 1.4550 X6CrNiNb18-10 | Nb stabilized weld/thermal applications | Cr 17–19; Ni 9–13; Nb controlled |
| 904L | N08904 | 1.4539 X1NiCrMoCu25-20-5 | high alloy austenitic; acid service | Cr 19–23; Ni 23–28; Mo 4–5; Cu 1–2 |
The chemistry column gives orientation ranges rounded from widely used specifications; acceptance requires the precise grade and edition’s chemical tables, product analysis tolerances and any agreed dual certification. EN variants under one US commercial name may have nonidentical nickel or molybdenum bounds.
400 series stainless grade register
| AISI / trade | UNS | EN screening cross-reference | Main tube relevance | Indicative chemistry, not acceptance limits |
|---|---|---|---|---|
| 405 | S40500 | 1.4002 X6CrAl13 | Al-alloyed ferritic stainless; distinct from coated steel | Cr 11.5–14.5; Al 0.10–0.30 |
| 409 | S40900 | 1.4512 X2CrTi12 | Ti stabilized; exhaust components | Cr 10.5–11.75; C ≤0.08; Ti stabilization |
| 409L | S40910 / EN variant | 1.4512 comparison | low-C exhaust; check grade-specific producer chemistry | Exact chemistry depends designation |
| 410 | S41000 | 1.4006 X12Cr13 | martensitic; may be heat treated | Cr 11.5–13.5; C ≤0.15 |
| 410S | S41008 | 1.4000 X6Cr13 | low-C ferritic counterpart | Cr 11.5–13.5; C ≤0.08 |
| 420 | S42000 | 1.4021 / 1.4028 variants | martensitic; wear/hardness applications | Cr 12–14; C varies materially |
| 430 | S43000 | 1.4016 X6Cr17 | 17% chromium; household/ducting | Cr 16–18; Ni not specified as alloy addition |
| 430Ti | varies | 1.4510/1.4520 comparison only | stabilized ferritic; specify exact designation | Cr ~16–18; Ti controlled |
| 434 | S43400 | 1.4113 X6CrMo17-1 | Mo-bearing ferritic corrosion upgrade | Cr 16–18; Mo ~0.75–1.25 |
| 436 | S43600 | 1.4526 comparison | Mo-bearing and stabilized exhaust option | Cr 16–18; Mo ~0.75–1.25 |
| 439 | S43035 | 1.4510 X3CrTi17 | Ti stabilized; exhaust and exchangers | Cr 17–19; Ti controlled |
| 441 | S43940 / S43932 | 1.4509 X2CrTiNb18 | dual stabilized Ti+Nb; elevated-temp exhaust | Cr ~17.5–18.5; Ti+Nb controlled |
| 444 | S44400 | 1.4521 X2CrMoTi18-2 | Mo-bearing ferritic; high corrosion resistance | Cr 17–20; Mo 1.75–2.5 |
| 446 | S44600 | 1.4749 comparison | high-Cr oxidation resistance | Cr 23–27 |
The 400 series spans ferritic and martensitic alloys. 409, 430, 439, 441 and 444 are ferritic; 410 and many 420 variants are martensitic. They cannot be substituted by series number alone. Stabilization is essential to welding and heat-resistance performance.
Special study 409AL and aluminized stainless
Two different uses of a similar name
In exhaust purchasing, “409AL”, “409 Aluminized” or “aluminized 409” commonly describes a 409 ferritic stainless substrate with hot-dip Al–Si coating (often Type 1), supplied as coated strip under ASTM A463/A463M or an agreed equivalent manufacturing specification. In other metallurgical contexts “409Al” may designate an aluminum-stabilized ferritic alloy rather than a surface-coated product. The suffix AL is not a safe stand-alone specification or universally standardized UNS grade.
| Check | Required PO or MTC statement |
|---|---|
| Substrate | UNS S40900 / other explicitly specified 409 family grade; separate heat analysis |
| Coating | Al–Si Type 1 vs pure-Al Type 2; applicable sheet standard or mill technical specification |
| Coating mass | Exact T1 / T1M or EN AS designation, total-both-sides vs per-side convention |
| Finished tube | Tube standard, process (ERW, TIG/laser), OD, wall and length tolerances |
| Weld | Treatment of weld seam and local coating loss; corrosion qualification if required |
| Verification | Coating mass/thickness; adhesion; substrate PMI; tube dimensional and leak tests |
A 409 substrate with aluminized coating is neither plain aluminized carbon steel nor bare 409 stainless. The coating may be damaged or absent at the weld seam and cut ends; agree on treatment and service testing. The producer should specify coating condition after tube forming, not only before it.
Chinese mill certificate checklist by material
| Product group | Minimum mill document field | Additional decisive check |
|---|---|---|
| Carbon Q235/Q355 | Heat, chemical analysis, tensile, impact category if ordered | Exact structural steel quality and thickness interval |
| Cold rolled DC01–DC06 | Re/Rp, Rm, A80, r and n where applicable | Surface finish, formability, strain aging |
| DX54D+AS120 | Substrate grade and coating designation and mass | Al–Si coating adherence and after-forming condition |
| 300 series SS | GB/T 20878 chemistry + flat-product standard + surface | Weld sensitization, PMI, solution anneal when relevant |
| 400 series SS | Cr/C/N/Ti/Nb/Mo chemistry, annealed temper | Weld HAZ, embrittlement and surface oxidation |
| 409AL | Identify whether coated 409 stainless or Al-stabilized grade | Separate substrate chemistry and coating evidence |
Tube purchase-order specification matrix
| Field | What an engineering inquiry or PO must state |
|---|---|
| Product | Welded round tube; intended mechanical, exhaust, heat-exchanger or pressure duty |
| Base grade | Exact material designation and source sheet/strip standard + edition |
| Coating | None / Al–Si / Al / Zn–Al; mass, type, both-face convention, coil condition |
| Tube standard | Applicable finished-product norm and edition; do not infer from strip grade |
| Dimensions | OD x nominal wall x cut length; tolerances, eccentricity, straightness, ovality |
| Production | HF-ERW / laser / TIG; weld-bead treatment; anneal/pickling/passivation if relevant |
| Verification | Chemistry, tensile or hardness, flattening/flaring/bend, leak/eddy/UT where applicable |
| Certification | EN 10204 3.1 or other agreed inspection certificate; heat/coil/tube traceability |
| Packing | Blue-wrapped bundles, without pallet/sleeve/slings if requested; moisture protection |
Tube manufacturing and acceptance checks
Coil receipt
Record heat number, coil number, coating face/mass, thickness, tensile condition and supplier MTC. A tube made from a compliant coil is not automatically a compliant tube.
Slitting and forming
Confirm strip edge condition, strip width, springback, seam orientation, and coating crack tolerance. High-strength sheet may have limited formability.
Weld process
Identify HF-ERW, TIG or laser; assess weld speed and heat input, seam bead and heat-affected region. High-Cr ferritic tubes need controlled welding and may require post-weld treatment.
Dimensional checks
Measure OD, nominal and minimum wall, out-of-roundness, length, straightness, end squareness and bend/ovality where specified. Use the actual tube standard tolerances.
Nondestructive/leak testing
Apply the specific test prescribed or agreed for the product: eddy-current, ultrasonic, pneumatic or hydrostatic. An inspection technology is not a substitute for the required acceptance level.
Marking and documentation
Record manufacturer, standard, grade, size, batch/heat and inspection results. Any claim to ASTM, EN or GOST should be supported by all relevant mandatory tests.
Primary sources
https://openstd.samr.gov.cn/bzgk/std/newGbInfo?hcno=192F05BCCC66349370A28EDF0CC742EA
https://openstd.samr.gov.cn/bzgk/std/newGbInfo?hcno=9ABAE7D4AB43B1B3F78BAF65B9C6291F
https://openstd.samr.gov.cn/bzgk/std/newGbInfo?hcno=8B23C177DDD1CF1F010206D48DAAC71D
https://openstd.samr.gov.cn/bzgk/std/newGbInfo?hcno=D70887EA9D2E0DEDA308A4177EE4B81C
https://openstd.samr.gov.cn/bzgk/std/newGbInfo?hcno=9F80F33DB9597FB0C628094B1525042F