Shaped for Precision. Built for Industry.

Materials Standards

European Steel and Tube Standards

EN reference for forming steels, Al–Si coatings and stainless tube products

Technical procurement and manufacturing reference | 17 November 2026 | Units: mm, MPa, mass % unless stated otherwise

Purpose and interpretation

This guide connects raw-material/coil designations with specifications for finished tubes. A grade alone does not define a compliant tube: the purchase order must also identify product form, applicable edition, dimensions, tolerance class, delivery condition, testing, inspection and documentation. Tables are curated commercial grade families, not a reproduction of copyrighted standards or an assertion that every grade ever standardized is included.

Important conformity principle

A comparison such as ASTM 304 ≈ EN 1.4301 ≈ a GOST chromium–nickel grade is a screening aid only. Chemical limits, deoxidation, stabilization, mechanical requirements, permitted processes, heat treatment and tests can differ. Never print an untested alternative standard on an MTC, and never treat a flat-sheet standard as finished-tube certification.

Standards register and applicability

StandardScopePractical applicability
EN 10130Cold-rolled low-carbon flat steel for cold formingDC01–DC06 family, mechanical/formability
EN 10131Size and shape tolerances for cold-rolled uncoated sheetThickness, width, flatness
EN 10025-2Hot-rolled nonalloy structural steelsS235JR/J0/J2, S275, S355
EN 10111Continuously hot-rolled low-carbon sheet for cold formingDD11–DD14
EN 10346Continuously hot-dip coated steel flat productsDX51D–DX56D, S grades, coating codes including AS
EN 10143Dimensional tolerances on continuously hot-dip coated flat productsRelevant to EN 10346 coil
EN 10088-1List of stainless steelsDesignation and composition reference
EN 10088-2Stainless sheet/plate/strip for general purposesSubstrate property/condition
EN 10028-7Stainless flat products for pressure purposesPressure flat-product specification
EN 10217-1Welded tubes for pressure purposes, nonalloy steelPressure-qualified welded carbon tubes
EN 10217-7Welded stainless tubes for pressure purposes300/400 stainless, specified tests
EN 10216-1Seamless nonalloy steel pressure tubesSeamless route
EN 10305-1Seamless cold-drawn precision tubesPrecision dimensional requirements
EN 10305-2Welded cold-drawn precision tubesPrecision welded and drawn
EN 10305-3Welded cold-sized precision tubesE155–E355 family
EN 10305-5Welded cold-sized square/rectangular precision tubesProfile tube variants
EN 10219-1/-2Cold-formed welded structural hollow sectionsS235JRH / S355J2H etc.
EN 10210-1/-2Hot-finished structural hollow sectionsDifferent manufacturing/dimensional rules
EN 10296-1Welded round steel tubes for mechanical/general engineeringNonalloy and alloy steels
EN 10296-2Welded round stainless tubes for mechanical engineeringStainless route
EN 10297-1/-2Seamless round mechanical engineering tubesCarbon / stainless variants
EN 10204Metallic-product inspection document types2.2 / 3.1 / 3.2 certificates
EN ISO 10893NDT of steel tubes seriesPart-specific UT/eddy/leak methods and levels

Mild and structural steel families

GradeSteel number / specificationPurposeInterpretation
DC011.0330Cold-rolled commercial formingRm approx 270–410 MPa; yield varies by delivery
DC031.0347Drawing-quality cold-rolled sheetImproved formability over DC01
DC041.0338Deep drawingLow yield, higher elongation
DC051.0312Extra deep drawingHigh-formability substrate
DC061.0873Special deep drawingVery low interstitial steel, aging resistance
DD111.0332Hot-rolled forming stripUncoated, not a finished tube spec
DD121.0398Hot-rolled drawing stripMore forming capability
DD13 / DD141.0335 / 1.0389Higher hot-rolled drawing gradesVerify edition and mechanical values
S235JR1.0038Structural hot-rolledNominal min yield 235 MPa at t ≤16 mm
S275JR1.0044Structural hot-rolledNominal min yield 275 MPa at t ≤16 mm
S355JR / J21.0045 / 1.0577Higher-strength structuralNominal min yield 355 MPa at t ≤16 mm
E155 / E195 / E235 / E275 / E355EN 10305 familyPrecision tube steelE-number denotes nominal strength class; supply condition changes values
P235TR1 / TR2EN 10217-1Welded pressure tubesTest category distinguishes obligations
P265TR1 / TR2EN 10217-1Higher-pressure strength gradeNot comparable to S235 solely by numeral

DC01 to DC06 mechanical property comparison

As forming demand increases from DC01 to DC06, specified yield strength generally decreases and the plastic strain ratio and elongation requirements become more demanding. Values vary with material thickness, test specimen orientation and applicable edition; use the grade-specific EN 10130 tables. DC02 is a legacy/historical designation and should not be assumed currently orderable under a new EN 10130 certificate.

Al–Si hot-dip coated steel grades

DesignationNumber or coating massTechnical meaning
DX51D1.0917 (2026 edition)Commercial forming coated substrate
DX52D1.0918 (2026 edition)Drawing substrate
DX53D1.0951 (2026 edition)Deep drawing
DX54D1.0952 (2026 edition)Special deep drawing
DX55D1.0962 (2026 edition)Enhanced deep drawing
DX56D1.0963 (2026 edition)Extra deep drawing
S220GD / S250GD1.0241 / 1.0242Structural coated grades
S280GD / S320GD1.0244 / 1.0250Structural coated grades
S350GD / S390GD1.0529 / 1.0238Higher-strength coated grades
S420GD / S450GD / S550GDcheck current editionHigh-strength coated steel; verify compatibility with AS
AS8080 g/m² total both sidesAl–Si coating; nominally ~40/40 per face if symmetric
AS120120 g/m² total both sidesAl–Si coating; 60/60 nominal if symmetric
AS150150 g/m² total both sidesAl–Si coating; 75/75 nominal if symmetric
AS200 / AS250 / AS300higher coating mass optionsVerify listing/availability and effect on forming

Why DX54D plus AS120 is a complete coil designation

DX54D defines the low-carbon substrate and forming quality; AS120 defines aluminum–silicon coating mass, nominally 120 g/m² total on two sides. EN 10346 provides the material/coating specification while EN 10143 governs applicable dimensional tolerances. A tube made from this coil must separately meet its chosen finished tube specification.

Coating nomenclature warning

AS (aluminum–silicon) is not AZ (aluminum–zinc), Z (zinc) or ZM (zinc–magnesium). All are metallic-coated flat products but their corrosion and high-temperature behavior differ. Coating mass, adhesion, external surface, seam continuity and forming effects must be checked separately.

300 series stainless grade register

AISI / tradeUNSEN screening cross-referenceMain tube relevanceIndicative chemistry, not acceptance limits
301S301001.4310 X10CrNi18-8austenitic; high work hardening; formed partsCr 16–18; Ni 6–8; C ≤0.15
302S302001.4319 (comparison only)austenitic; higher C than 304Cr 17–19; Ni 8–10; C ≤0.15
303S303001.4305 X8CrNiS18-9free-machining; sulfur; poor welding choiceCr 17–19; Ni 8–10; S ≥0.15
304S304001.4301 X5CrNi18-10general welded tube and fabricationCr 18–20; Ni 8–10.5; C ≤0.08
304LS304031.4307 / 1.4306lower carbon; welded assembliesCr 18–20; Ni 8–12; C ≤0.03
304HS304091.4948 (check product)elevated temperature; controlled carbonC 0.04–0.10; Cr 18–20; Ni 8–11
305S305001.4303 X4CrNi18-12deep forming; higher nickelCr 17–19; Ni 11–13
309SS309081.4833 X12CrNi23-13heat oxidation serviceCr 22–24; Ni 12–15; C ≤0.08
310SS310081.4845 X8CrNi25-21heat-resistant high chromium nickelCr 24–26; Ni 19–22; C ≤0.08
316S316001.4401 X5CrNiMo17-12-2molybdenum for chloride resistanceCr 16–18; Ni 10–14; Mo 2–3
316LS316031.4404 / 1.4432 / 1.4435welded chemical and hygienic tubesC ≤0.03; Cr 16–18; Mo 2–3
316TiS316351.4571 X6CrNiMoTi17-12-2Ti stabilized; hot serviceCr 16.5–18.5; Ni 10.5–13.5; Mo 2–2.5
317LS317031.4438 (comparison only)higher Mo; aggressive serviceCr 18–20; Ni 11–15; Mo 3–4
321S321001.4541 X6CrNiTi18-10Ti stabilized exhaust and heatCr 17–19; Ni 9–12; Ti controlled
347S347001.4550 X6CrNiNb18-10Nb stabilized weld/thermal applicationsCr 17–19; Ni 9–13; Nb controlled
904LN089041.4539 X1NiCrMoCu25-20-5high alloy austenitic; acid serviceCr 19–23; Ni 23–28; Mo 4–5; Cu 1–2

The chemistry column gives orientation ranges rounded from widely used specifications; acceptance requires the precise grade and edition’s chemical tables, product analysis tolerances and any agreed dual certification. EN variants under one US commercial name may have nonidentical nickel or molybdenum bounds.

400 series stainless grade register

AISI / tradeUNSEN screening cross-referenceMain tube relevanceIndicative chemistry, not acceptance limits
405S405001.4002 X6CrAl13Al-alloyed ferritic stainless; distinct from coated steelCr 11.5–14.5; Al 0.10–0.30
409S409001.4512 X2CrTi12Ti stabilized; exhaust componentsCr 10.5–11.75; C ≤0.08; Ti stabilization
409LS40910 / EN variant1.4512 comparisonlow-C exhaust; check grade-specific producer chemistryExact chemistry depends designation
410S410001.4006 X12Cr13martensitic; may be heat treatedCr 11.5–13.5; C ≤0.15
410SS410081.4000 X6Cr13low-C ferritic counterpartCr 11.5–13.5; C ≤0.08
420S420001.4021 / 1.4028 variantsmartensitic; wear/hardness applicationsCr 12–14; C varies materially
430S430001.4016 X6Cr1717% chromium; household/ductingCr 16–18; Ni not specified as alloy addition
430Tivaries1.4510/1.4520 comparison onlystabilized ferritic; specify exact designationCr ~16–18; Ti controlled
434S434001.4113 X6CrMo17-1Mo-bearing ferritic corrosion upgradeCr 16–18; Mo ~0.75–1.25
436S436001.4526 comparisonMo-bearing and stabilized exhaust optionCr 16–18; Mo ~0.75–1.25
439S430351.4510 X3CrTi17Ti stabilized; exhaust and exchangersCr 17–19; Ti controlled
441S43940 / S439321.4509 X2CrTiNb18dual stabilized Ti+Nb; elevated-temp exhaustCr ~17.5–18.5; Ti+Nb controlled
444S444001.4521 X2CrMoTi18-2Mo-bearing ferritic; high corrosion resistanceCr 17–20; Mo 1.75–2.5
446S446001.4749 comparisonhigh-Cr oxidation resistanceCr 23–27

The 400 series spans ferritic and martensitic alloys. 409, 430, 439, 441 and 444 are ferritic; 410 and many 420 variants are martensitic. They cannot be substituted by series number alone. Stabilization is essential to welding and heat-resistance performance.

Special study 409AL and aluminized stainless

Two different uses of a similar name

In exhaust purchasing, “409AL”, “409 Aluminized” or “aluminized 409” commonly describes a 409 ferritic stainless substrate with hot-dip Al–Si coating (often Type 1), supplied as coated strip under ASTM A463/A463M or an agreed equivalent manufacturing specification. In other metallurgical contexts “409Al” may designate an aluminum-stabilized ferritic alloy rather than a surface-coated product. The suffix AL is not a safe stand-alone specification or universally standardized UNS grade.

CheckRequired PO or MTC statement
SubstrateUNS S40900 / other explicitly specified 409 family grade; separate heat analysis
CoatingAl–Si Type 1 vs pure-Al Type 2; applicable sheet standard or mill technical specification
Coating massExact T1 / T1M or EN AS designation, total-both-sides vs per-side convention
Finished tubeTube standard, process (ERW, TIG/laser), OD, wall and length tolerances
WeldTreatment of weld seam and local coating loss; corrosion qualification if required
VerificationCoating mass/thickness; adhesion; substrate PMI; tube dimensional and leak tests

A 409 substrate with aluminized coating is neither plain aluminized carbon steel nor bare 409 stainless. The coating may be damaged or absent at the weld seam and cut ends; agree on treatment and service testing. The producer should specify coating condition after tube forming, not only before it.

EN 10130 uncoated cold-rolled sheet detailed limits

GradeC max %Mn max %P / S max %Yield MPaTensile MPaA80 min %
DC010.120.600.045 / 0.045140–280270–41028
DC030.100.450.035 / 0.035140–240270–37034
DC040.080.400.030 / 0.030140–210270–35038
DC050.060.350.025 / 0.025140–180270–33040
DC060.020.250.020 / 0.020140–180270–33041

Reference basis: EN 10130:2006 grade tables, as reproduced in steelmaker technical literature. Applies to defined thickness/orientation/test lengths and delivery time; check contractual edition and thickness adjustments. DC06 is an interstitial-free grade and other Ti specifications may apply. These are sheet limits, not tube limits.

EN 10346 Al–Si substrate mechanical limits

Grade + coatingYield MPaTensile MPaA80 minimum %Notes
DX51D+ASnot specified270–50022General forming; coating-dependent
DX52D+AS140–300270–42026Drawing
DX53D+AS140–260270–38030Deep drawing
DX54D+AS120–220260–35034AS-specific elongation condition
DX55D+AS140–240270–37030AS-specific substrate
DX56D+AS120–180260–35039AS-specific high forming quality

Figures are EN 10346:2015-era AS-specific longitudinal/transverse test-condition reference values as published by steel producers and historical standards previews. EN 10346:2026 has been published; confirm its new edition, test direction, thickness exceptions and grade steel numbers before certification. EN 10346:2026 uses 1.0917 DX51D, 1.0918 DX52D, 1.0951 DX53D, 1.0952 DX54D, 1.0962 DX55D and 1.0963 DX56D; older tables used different numbers.

EN Al–Si coating mass and geometric interpretation

CoatingNominal minimum total coating massApproximate per side if symmetricApproximate combined two-face thickness
AS8080 g/m²40 g/m²~30 µm
AS120120 g/m²60 g/m²~45 µm
AS150150 g/m²75 g/m²~56 µm

Approximate coating thickness calculated from total mass ÷ Al–Si alloy density (~2.7 g/cm³), split evenly between two faces. This is a geometric conversion, NOT EN 10346 single-spot minimum thickness; the required laboratory coating-mass sampling, minimum triple-spot and single-spot criteria must be consulted in the edition specified.

Individual stainless steel technical specification sheets

301 stainless steel S30100

Specification fieldTechnical requirement / engineering guidance
Chemical compositionCr 16–18; Ni 6–8; C ≤0.15
Mechanical propertiesCold-worked tempers can increase strength greatly; annealed values must not be applied to half-hard/full-hard strip.
Supply and metallurgical conditionAustenitic; confirm solution-annealed vs cold-worked temper, surface finish, EN number (1.4310 X10CrNi18-8) and corrosion exposure.
Tube production considerationsStrong work hardening; control rolling and tube-forming strain.
Inspection, test and certificateUse EN 10296-2 / EN 10217-7 as applicable tube-product specification matching application. Test chemistry/PMI, tensile as applicable, dimensions, weld integrity, surface and corrosion requirements; MTC to state grade, heat and precise standard edition.
Basis / precisionIndicative chemistry, not a complete mandatory heat/product analysis; strength examples refer to selected annealed flat products and require standard verification.

302 stainless steel S30200

Specification fieldTechnical requirement / engineering guidance
Chemical compositionCr 17–19; Ni 8–10; C ≤0.15
Mechanical propertiesMechanical properties depend on annealed or cold-worked temper.
Supply and metallurgical conditionAustenitic; confirm solution-annealed vs cold-worked temper, surface finish, EN number (1.4319 (comparison only)) and corrosion exposure.
Tube production considerationsHigher carbon means evaluate weld sensitization.
Inspection, test and certificateUse EN 10296-2 / EN 10217-7 as applicable tube-product specification matching application. Test chemistry/PMI, tensile as applicable, dimensions, weld integrity, surface and corrosion requirements; MTC to state grade, heat and precise standard edition.
Basis / precisionIndicative chemistry, not a complete mandatory heat/product analysis; strength examples refer to selected annealed flat products and require standard verification.

303 stainless steel S30300

Specification fieldTechnical requirement / engineering guidance
Chemical compositionCr 17–19; Ni 8–10; S ≥0.15
Mechanical propertiesMechanical strength depends on product form and temper.
Supply and metallurgical conditionAustenitic; confirm solution-annealed vs cold-worked temper, surface finish, EN number (1.4305 X8CrNiS18-9) and corrosion exposure.
Tube production considerationsSulfur addition improves machinability but reduces fusion-weld suitability.
Inspection, test and certificateUse EN 10296-2 / EN 10217-7 as applicable tube-product specification matching application. Test chemistry/PMI, tensile as applicable, dimensions, weld integrity, surface and corrosion requirements; MTC to state grade, heat and precise standard edition.
Basis / precisionIndicative chemistry, not a complete mandatory heat/product analysis; strength examples refer to selected annealed flat products and require standard verification.

304 stainless steel S30400

Specification fieldTechnical requirement / engineering guidance
Chemical compositionCr 18–20; Ni 8–10.5; C ≤0.08
Mechanical propertiesTypical solution-annealed plate/sheet minimum: Rp0.2 ~205 MPa; Rm ~515 MPa; elongation ~40% under common ASTM flat-product conditions. These figures are NOT universal finished-tube limits.
Supply and metallurgical conditionAustenitic; confirm solution-annealed vs cold-worked temper, surface finish, EN number (1.4301 X5CrNi18-10) and corrosion exposure.
Tube production considerationsTIG/laser or qualified ERW; assess seam corrosion, ID bead, and sensitization.
Inspection, test and certificateUse EN 10296-2 / EN 10217-7 as applicable tube-product specification matching application. Test chemistry/PMI, tensile as applicable, dimensions, weld integrity, surface and corrosion requirements; MTC to state grade, heat and precise standard edition.
Basis / precisionIndicative chemistry, not a complete mandatory heat/product analysis; strength examples refer to selected annealed flat products and require standard verification.

304L stainless steel S30403

Specification fieldTechnical requirement / engineering guidance
Chemical compositionCr 18–20; Ni 8–12; C ≤0.03
Mechanical propertiesTypical annealed flat-product minima often Rp0.2 ~170 MPa, Rm ~485 MPa, A ~40%; verify actual product-standard edition.
Supply and metallurgical conditionAustenitic; confirm solution-annealed vs cold-worked temper, surface finish, EN number (1.4307 / 1.4306) and corrosion exposure.
Tube production considerationsLow carbon preferred for welded parts; 304/304L dual certificate requires both chemistries and all mechanical requirements.
Inspection, test and certificateUse EN 10296-2 / EN 10217-7 as applicable tube-product specification matching application. Test chemistry/PMI, tensile as applicable, dimensions, weld integrity, surface and corrosion requirements; MTC to state grade, heat and precise standard edition.
Basis / precisionIndicative chemistry, not a complete mandatory heat/product analysis; strength examples refer to selected annealed flat products and require standard verification.

304H stainless steel S30409

Specification fieldTechnical requirement / engineering guidance
Chemical compositionC 0.04–0.10; Cr 18–20; Ni 8–11
Mechanical propertiesHigh-temperature grades require carbon control and elevated-temperature design values.
Supply and metallurgical conditionAustenitic; confirm solution-annealed vs cold-worked temper, surface finish, EN number (1.4948 (check product)) and corrosion exposure.
Tube production considerationsNot interchangeable with 304L; confirm thermal service and heat treatment.
Inspection, test and certificateUse EN 10296-2 / EN 10217-7 as applicable tube-product specification matching application. Test chemistry/PMI, tensile as applicable, dimensions, weld integrity, surface and corrosion requirements; MTC to state grade, heat and precise standard edition.
Basis / precisionIndicative chemistry, not a complete mandatory heat/product analysis; strength examples refer to selected annealed flat products and require standard verification.

305 stainless steel S30500

Specification fieldTechnical requirement / engineering guidance
Chemical compositionCr 17–19; Ni 11–13
Mechanical propertiesCold-forming optimized; yield/tensile depend on condition.
Supply and metallurgical conditionAustenitic; confirm solution-annealed vs cold-worked temper, surface finish, EN number (1.4303 X4CrNi18-12) and corrosion exposure.
Tube production considerationsExcellent deep formability; check availability of tube coil.
Inspection, test and certificateUse EN 10296-2 / EN 10217-7 as applicable tube-product specification matching application. Test chemistry/PMI, tensile as applicable, dimensions, weld integrity, surface and corrosion requirements; MTC to state grade, heat and precise standard edition.
Basis / precisionIndicative chemistry, not a complete mandatory heat/product analysis; strength examples refer to selected annealed flat products and require standard verification.

309S stainless steel S30908

Specification fieldTechnical requirement / engineering guidance
Chemical compositionCr 22–24; Ni 12–15; C ≤0.08
Mechanical propertiesHeat-resistant austenitic; strength is condition and temperature dependent.
Supply and metallurgical conditionAustenitic; confirm solution-annealed vs cold-worked temper, surface finish, EN number (1.4833 X12CrNi23-13) and corrosion exposure.
Tube production considerationsOxidation/thermal cycling design matters more than generic room-temperature strength.
Inspection, test and certificateUse EN 10296-2 / EN 10217-7 as applicable tube-product specification matching application. Test chemistry/PMI, tensile as applicable, dimensions, weld integrity, surface and corrosion requirements; MTC to state grade, heat and precise standard edition.
Basis / precisionIndicative chemistry, not a complete mandatory heat/product analysis; strength examples refer to selected annealed flat products and require standard verification.

310S stainless steel S31008

Specification fieldTechnical requirement / engineering guidance
Chemical compositionCr 24–26; Ni 19–22; C ≤0.08
Mechanical propertiesHeat-resistant austenitic; check high-temperature creep/oxidation rating separately.
Supply and metallurgical conditionAustenitic; confirm solution-annealed vs cold-worked temper, surface finish, EN number (1.4845 X8CrNi25-21) and corrosion exposure.
Tube production considerationsHigh alloy weld consumable and thermal expansion considerations.
Inspection, test and certificateUse EN 10296-2 / EN 10217-7 as applicable tube-product specification matching application. Test chemistry/PMI, tensile as applicable, dimensions, weld integrity, surface and corrosion requirements; MTC to state grade, heat and precise standard edition.
Basis / precisionIndicative chemistry, not a complete mandatory heat/product analysis; strength examples refer to selected annealed flat products and require standard verification.

316 stainless steel S31600

Specification fieldTechnical requirement / engineering guidance
Chemical compositionCr 16–18; Ni 10–14; Mo 2–3
Mechanical propertiesCommon annealed flat-product minima: Rp0.2 ~205 MPa, Rm ~515 MPa, A ~40%; do not apply to every tube product.
Supply and metallurgical conditionAustenitic; confirm solution-annealed vs cold-worked temper, surface finish, EN number (1.4401 X5CrNiMo17-12-2) and corrosion exposure.
Tube production considerationsMo enhances pitting resistance; not immune to chloride stress corrosion.
Inspection, test and certificateUse EN 10296-2 / EN 10217-7 as applicable tube-product specification matching application. Test chemistry/PMI, tensile as applicable, dimensions, weld integrity, surface and corrosion requirements; MTC to state grade, heat and precise standard edition.
Basis / precisionIndicative chemistry, not a complete mandatory heat/product analysis; strength examples refer to selected annealed flat products and require standard verification.

316L stainless steel S31603

Specification fieldTechnical requirement / engineering guidance
Chemical compositionC ≤0.03; Cr 16–18; Mo 2–3
Mechanical propertiesCommon annealed flat-product minima: Rp0.2 ~170 MPa, Rm ~485 MPa, A ~40%; verify product-specific requirements.
Supply and metallurgical conditionAustenitic; confirm solution-annealed vs cold-worked temper, surface finish, EN number (1.4404 / 1.4432 / 1.4435) and corrosion exposure.
Tube production considerationsLower carbon for welded corrosion service; surface passivation may be specified.
Inspection, test and certificateUse EN 10296-2 / EN 10217-7 as applicable tube-product specification matching application. Test chemistry/PMI, tensile as applicable, dimensions, weld integrity, surface and corrosion requirements; MTC to state grade, heat and precise standard edition.
Basis / precisionIndicative chemistry, not a complete mandatory heat/product analysis; strength examples refer to selected annealed flat products and require standard verification.

316Ti stainless steel S31635

Specification fieldTechnical requirement / engineering guidance
Chemical compositionCr 16.5–18.5; Ni 10.5–13.5; Mo 2–2.5
Mechanical propertiesCondition, temperature and specimen direction determine applicable mechanical minima.
Supply and metallurgical conditionAustenitic; confirm solution-annealed vs cold-worked temper, surface finish, EN number (1.4571 X6CrNiMoTi17-12-2) and corrosion exposure.
Tube production considerationsTi stabilized; specify solution treatment and avoid assuming same chemistry as 316L.
Inspection, test and certificateUse EN 10296-2 / EN 10217-7 as applicable tube-product specification matching application. Test chemistry/PMI, tensile as applicable, dimensions, weld integrity, surface and corrosion requirements; MTC to state grade, heat and precise standard edition.
Basis / precisionIndicative chemistry, not a complete mandatory heat/product analysis; strength examples refer to selected annealed flat products and require standard verification.

317L stainless steel S31703

Specification fieldTechnical requirement / engineering guidance
Chemical compositionCr 18–20; Ni 11–15; Mo 3–4
Mechanical propertiesHigher Mo chemistry; mechanical values require exact product specification.
Supply and metallurgical conditionAustenitic; confirm solution-annealed vs cold-worked temper, surface finish, EN number (1.4438 (comparison only)) and corrosion exposure.
Tube production considerationsCorrosion qualification should match chloride/acidity environment.
Inspection, test and certificateUse EN 10296-2 / EN 10217-7 as applicable tube-product specification matching application. Test chemistry/PMI, tensile as applicable, dimensions, weld integrity, surface and corrosion requirements; MTC to state grade, heat and precise standard edition.
Basis / precisionIndicative chemistry, not a complete mandatory heat/product analysis; strength examples refer to selected annealed flat products and require standard verification.

321 stainless steel S32100

Specification fieldTechnical requirement / engineering guidance
Chemical compositionCr 17–19; Ni 9–12; Ti controlled
Mechanical propertiesCommon annealed flat-product tensile minimum around 515 MPa; full yield/elongation require edition.
Supply and metallurgical conditionAustenitic; confirm solution-annealed vs cold-worked temper, surface finish, EN number (1.4541 X6CrNiTi18-10) and corrosion exposure.
Tube production considerationsTitanium stabilization and weld heat exposure make treatment critical.
Inspection, test and certificateUse EN 10296-2 / EN 10217-7 as applicable tube-product specification matching application. Test chemistry/PMI, tensile as applicable, dimensions, weld integrity, surface and corrosion requirements; MTC to state grade, heat and precise standard edition.
Basis / precisionIndicative chemistry, not a complete mandatory heat/product analysis; strength examples refer to selected annealed flat products and require standard verification.

347 stainless steel S34700

Specification fieldTechnical requirement / engineering guidance
Chemical compositionCr 17–19; Ni 9–13; Nb controlled
Mechanical propertiesStabilized Cr–Ni steel; property limits depend on standard and condition.
Supply and metallurgical conditionAustenitic; confirm solution-annealed vs cold-worked temper, surface finish, EN number (1.4550 X6CrNiNb18-10) and corrosion exposure.
Tube production considerationsNb stabilization; specify temperature cycling, weld process and test plan.
Inspection, test and certificateUse EN 10296-2 / EN 10217-7 as applicable tube-product specification matching application. Test chemistry/PMI, tensile as applicable, dimensions, weld integrity, surface and corrosion requirements; MTC to state grade, heat and precise standard edition.
Basis / precisionIndicative chemistry, not a complete mandatory heat/product analysis; strength examples refer to selected annealed flat products and require standard verification.

904L stainless steel N08904

Specification fieldTechnical requirement / engineering guidance
Chemical compositionCr 19–23; Ni 23–28; Mo 4–5; Cu 1–2
Mechanical propertiesHigh alloy austenitic; minimum properties are product- and condition-specific.
Supply and metallurgical conditionAustenitic; confirm solution-annealed vs cold-worked temper, surface finish, EN number (1.4539 X1NiCrMoCu25-20-5) and corrosion exposure.
Tube production considerationsHigh Ni/Mo/Cu content; demanding weld qualification and PMI.
Inspection, test and certificateUse EN 10296-2 / EN 10217-7 as applicable tube-product specification matching application. Test chemistry/PMI, tensile as applicable, dimensions, weld integrity, surface and corrosion requirements; MTC to state grade, heat and precise standard edition.
Basis / precisionIndicative chemistry, not a complete mandatory heat/product analysis; strength examples refer to selected annealed flat products and require standard verification.

405 stainless steel S40500

Specification fieldTechnical requirement / engineering guidance
Chemical compositionCr 11.5–14.5; Al 0.10–0.30
Mechanical propertiesMechanical requirements must be selected from the correct stainless flat or tube product standard and heat-treatment condition; no generic 400-series minimum applies.
Supply and metallurgical conditionAl-alloyed ferritic stainless; distinct from coated steel; match exact UNS and EN designation (1.4002 X6CrAl13), anneal/temper, surface finish and stabilization.
Tube production considerationsFerritic alloys require attention to weld heat-affected-zone toughness, stabilizers and bead finish; martensitic grades may require heat treatment and hardness control.
Inspection, test and certificateOrder to EN 10296-2 / EN 10217-7 as applicable applicable tube norm; chemical analysis, dimensional checks, hardness/tensile where required, weld NDT or leak test, traceability and coating inspection if aluminized.
Basis / precisionChemistry overview and indicative industry property bands; exact pass/fail limits reside in the named edition and product form.

409 stainless steel S40900

Specification fieldTechnical requirement / engineering guidance
Chemical compositionCr 10.5–11.75; C ≤0.08; Ti stabilization
Mechanical propertiesTypical annealed mechanical properties: yield roughly 170–240 MPa, tensile 380–480 MPa, elongation ~20–30%; commercial supplier typicals, not acceptance minima.
Supply and metallurgical conditionTi stabilized; exhaust components; match exact UNS and EN designation (1.4512 X2CrTi12), anneal/temper, surface finish and stabilization.
Tube production considerationsFerritic alloys require attention to weld heat-affected-zone toughness, stabilizers and bead finish; martensitic grades may require heat treatment and hardness control.
Inspection, test and certificateOrder to EN 10296-2 / EN 10217-7 as applicable applicable tube norm; chemical analysis, dimensional checks, hardness/tensile where required, weld NDT or leak test, traceability and coating inspection if aluminized.
Basis / precisionChemistry overview and indicative industry property bands; exact pass/fail limits reside in the named edition and product form.

409L stainless steel S40910 / EN variant

Specification fieldTechnical requirement / engineering guidance
Chemical compositionExact chemistry depends designation
Mechanical propertiesLower interstitial chemistry; properties depend on exact UNS and strip anneal.
Supply and metallurgical conditionlow-C exhaust; check grade-specific producer chemistry; match exact UNS and EN designation (1.4512 comparison), anneal/temper, surface finish and stabilization.
Tube production considerationsFerritic alloys require attention to weld heat-affected-zone toughness, stabilizers and bead finish; martensitic grades may require heat treatment and hardness control.
Inspection, test and certificateOrder to EN 10296-2 / EN 10217-7 as applicable applicable tube norm; chemical analysis, dimensional checks, hardness/tensile where required, weld NDT or leak test, traceability and coating inspection if aluminized.
Basis / precisionChemistry overview and indicative industry property bands; exact pass/fail limits reside in the named edition and product form.

410 stainless steel S41000

Specification fieldTechnical requirement / engineering guidance
Chemical compositionCr 11.5–13.5; C ≤0.15
Mechanical propertiesMechanical requirements must be selected from the correct stainless flat or tube product standard and heat-treatment condition; no generic 400-series minimum applies.
Supply and metallurgical conditionmartensitic; may be heat treated; match exact UNS and EN designation (1.4006 X12Cr13), anneal/temper, surface finish and stabilization.
Tube production considerationsFerritic alloys require attention to weld heat-affected-zone toughness, stabilizers and bead finish; martensitic grades may require heat treatment and hardness control.
Inspection, test and certificateOrder to EN 10296-2 / EN 10217-7 as applicable applicable tube norm; chemical analysis, dimensional checks, hardness/tensile where required, weld NDT or leak test, traceability and coating inspection if aluminized.
Basis / precisionChemistry overview and indicative industry property bands; exact pass/fail limits reside in the named edition and product form.

410S stainless steel S41008

Specification fieldTechnical requirement / engineering guidance
Chemical compositionCr 11.5–13.5; C ≤0.08
Mechanical propertiesMechanical requirements must be selected from the correct stainless flat or tube product standard and heat-treatment condition; no generic 400-series minimum applies.
Supply and metallurgical conditionlow-C ferritic counterpart; match exact UNS and EN designation (1.4000 X6Cr13), anneal/temper, surface finish and stabilization.
Tube production considerationsFerritic alloys require attention to weld heat-affected-zone toughness, stabilizers and bead finish; martensitic grades may require heat treatment and hardness control.
Inspection, test and certificateOrder to EN 10296-2 / EN 10217-7 as applicable applicable tube norm; chemical analysis, dimensional checks, hardness/tensile where required, weld NDT or leak test, traceability and coating inspection if aluminized.
Basis / precisionChemistry overview and indicative industry property bands; exact pass/fail limits reside in the named edition and product form.

420 stainless steel S42000

Specification fieldTechnical requirement / engineering guidance
Chemical compositionCr 12–14; C varies materially
Mechanical propertiesMechanical requirements must be selected from the correct stainless flat or tube product standard and heat-treatment condition; no generic 400-series minimum applies.
Supply and metallurgical conditionmartensitic; wear/hardness applications; match exact UNS and EN designation (1.4021 / 1.4028 variants), anneal/temper, surface finish and stabilization.
Tube production considerationsFerritic alloys require attention to weld heat-affected-zone toughness, stabilizers and bead finish; martensitic grades may require heat treatment and hardness control.
Inspection, test and certificateOrder to EN 10296-2 / EN 10217-7 as applicable applicable tube norm; chemical analysis, dimensional checks, hardness/tensile where required, weld NDT or leak test, traceability and coating inspection if aluminized.
Basis / precisionChemistry overview and indicative industry property bands; exact pass/fail limits reside in the named edition and product form.

430 stainless steel S43000

Specification fieldTechnical requirement / engineering guidance
Chemical compositionCr 16–18; Ni not specified as alloy addition
Mechanical propertiesTypical annealed yield roughly 205–310 MPa, tensile ~450–550 MPa, elongation ~20–30%; supplier typicals, not acceptance minima.
Supply and metallurgical condition17% chromium; household/ducting; match exact UNS and EN designation (1.4016 X6Cr17), anneal/temper, surface finish and stabilization.
Tube production considerationsFerritic alloys require attention to weld heat-affected-zone toughness, stabilizers and bead finish; martensitic grades may require heat treatment and hardness control.
Inspection, test and certificateOrder to EN 10296-2 / EN 10217-7 as applicable applicable tube norm; chemical analysis, dimensional checks, hardness/tensile where required, weld NDT or leak test, traceability and coating inspection if aluminized.
Basis / precisionChemistry overview and indicative industry property bands; exact pass/fail limits reside in the named edition and product form.

430Ti stainless steel varies

Specification fieldTechnical requirement / engineering guidance
Chemical compositionCr ~16–18; Ti controlled
Mechanical propertiesMechanical requirements must be selected from the correct stainless flat or tube product standard and heat-treatment condition; no generic 400-series minimum applies.
Supply and metallurgical conditionstabilized ferritic; specify exact designation; match exact UNS and EN designation (1.4510/1.4520 comparison only), anneal/temper, surface finish and stabilization.
Tube production considerationsFerritic alloys require attention to weld heat-affected-zone toughness, stabilizers and bead finish; martensitic grades may require heat treatment and hardness control.
Inspection, test and certificateOrder to EN 10296-2 / EN 10217-7 as applicable applicable tube norm; chemical analysis, dimensional checks, hardness/tensile where required, weld NDT or leak test, traceability and coating inspection if aluminized.
Basis / precisionChemistry overview and indicative industry property bands; exact pass/fail limits reside in the named edition and product form.

434 stainless steel S43400

Specification fieldTechnical requirement / engineering guidance
Chemical compositionCr 16–18; Mo ~0.75–1.25
Mechanical propertiesMechanical requirements must be selected from the correct stainless flat or tube product standard and heat-treatment condition; no generic 400-series minimum applies.
Supply and metallurgical conditionMo-bearing ferritic corrosion upgrade; match exact UNS and EN designation (1.4113 X6CrMo17-1), anneal/temper, surface finish and stabilization.
Tube production considerationsFerritic alloys require attention to weld heat-affected-zone toughness, stabilizers and bead finish; martensitic grades may require heat treatment and hardness control.
Inspection, test and certificateOrder to EN 10296-2 / EN 10217-7 as applicable applicable tube norm; chemical analysis, dimensional checks, hardness/tensile where required, weld NDT or leak test, traceability and coating inspection if aluminized.
Basis / precisionChemistry overview and indicative industry property bands; exact pass/fail limits reside in the named edition and product form.

436 stainless steel S43600

Specification fieldTechnical requirement / engineering guidance
Chemical compositionCr 16–18; Mo ~0.75–1.25
Mechanical propertiesMechanical requirements must be selected from the correct stainless flat or tube product standard and heat-treatment condition; no generic 400-series minimum applies.
Supply and metallurgical conditionMo-bearing and stabilized exhaust option; match exact UNS and EN designation (1.4526 comparison), anneal/temper, surface finish and stabilization.
Tube production considerationsFerritic alloys require attention to weld heat-affected-zone toughness, stabilizers and bead finish; martensitic grades may require heat treatment and hardness control.
Inspection, test and certificateOrder to EN 10296-2 / EN 10217-7 as applicable applicable tube norm; chemical analysis, dimensional checks, hardness/tensile where required, weld NDT or leak test, traceability and coating inspection if aluminized.
Basis / precisionChemistry overview and indicative industry property bands; exact pass/fail limits reside in the named edition and product form.

439 stainless steel S43035

Specification fieldTechnical requirement / engineering guidance
Chemical compositionCr 17–19; Ti controlled
Mechanical propertiesTypical annealed yield ~240–320 MPa, tensile ~415–520 MPa; check actual strip MTC.
Supply and metallurgical conditionTi stabilized; exhaust and exchangers; match exact UNS and EN designation (1.4510 X3CrTi17), anneal/temper, surface finish and stabilization.
Tube production considerationsFerritic alloys require attention to weld heat-affected-zone toughness, stabilizers and bead finish; martensitic grades may require heat treatment and hardness control.
Inspection, test and certificateOrder to EN 10296-2 / EN 10217-7 as applicable applicable tube norm; chemical analysis, dimensional checks, hardness/tensile where required, weld NDT or leak test, traceability and coating inspection if aluminized.
Basis / precisionChemistry overview and indicative industry property bands; exact pass/fail limits reside in the named edition and product form.

441 stainless steel S43940 / S43932

Specification fieldTechnical requirement / engineering guidance
Chemical compositionCr ~17.5–18.5; Ti+Nb controlled
Mechanical propertiesTypical annealed yield ~250–350 MPa, tensile ~430–550 MPa; check grade variant and coil certificate.
Supply and metallurgical conditiondual stabilized Ti+Nb; elevated-temp exhaust; match exact UNS and EN designation (1.4509 X2CrTiNb18), anneal/temper, surface finish and stabilization.
Tube production considerationsFerritic alloys require attention to weld heat-affected-zone toughness, stabilizers and bead finish; martensitic grades may require heat treatment and hardness control.
Inspection, test and certificateOrder to EN 10296-2 / EN 10217-7 as applicable applicable tube norm; chemical analysis, dimensional checks, hardness/tensile where required, weld NDT or leak test, traceability and coating inspection if aluminized.
Basis / precisionChemistry overview and indicative industry property bands; exact pass/fail limits reside in the named edition and product form.

444 stainless steel S44400

Specification fieldTechnical requirement / engineering guidance
Chemical compositionCr 17–20; Mo 1.75–2.5
Mechanical propertiesMechanical requirements must be selected from the correct stainless flat or tube product standard and heat-treatment condition; no generic 400-series minimum applies.
Supply and metallurgical conditionMo-bearing ferritic; high corrosion resistance; match exact UNS and EN designation (1.4521 X2CrMoTi18-2), anneal/temper, surface finish and stabilization.
Tube production considerationsFerritic alloys require attention to weld heat-affected-zone toughness, stabilizers and bead finish; martensitic grades may require heat treatment and hardness control.
Inspection, test and certificateOrder to EN 10296-2 / EN 10217-7 as applicable applicable tube norm; chemical analysis, dimensional checks, hardness/tensile where required, weld NDT or leak test, traceability and coating inspection if aluminized.
Basis / precisionChemistry overview and indicative industry property bands; exact pass/fail limits reside in the named edition and product form.

446 stainless steel S44600

Specification fieldTechnical requirement / engineering guidance
Chemical compositionCr 23–27
Mechanical propertiesMechanical requirements must be selected from the correct stainless flat or tube product standard and heat-treatment condition; no generic 400-series minimum applies.
Supply and metallurgical conditionhigh-Cr oxidation resistance; match exact UNS and EN designation (1.4749 comparison), anneal/temper, surface finish and stabilization.
Tube production considerationsFerritic alloys require attention to weld heat-affected-zone toughness, stabilizers and bead finish; martensitic grades may require heat treatment and hardness control.
Inspection, test and certificateOrder to EN 10296-2 / EN 10217-7 as applicable applicable tube norm; chemical analysis, dimensional checks, hardness/tensile where required, weld NDT or leak test, traceability and coating inspection if aluminized.
Basis / precisionChemistry overview and indicative industry property bands; exact pass/fail limits reside in the named edition and product form.

Tube purchase-order specification matrix

FieldWhat an engineering inquiry or PO must state
ProductWelded round tube; intended mechanical, exhaust, heat-exchanger or pressure duty
Base gradeExact material designation and source sheet/strip standard + edition
CoatingNone / Al–Si / Al / Zn–Al; mass, type, both-face convention, coil condition
Tube standardApplicable finished-product norm and edition; do not infer from strip grade
DimensionsOD x nominal wall x cut length; tolerances, eccentricity, straightness, ovality
ProductionHF-ERW / laser / TIG; weld-bead treatment; anneal/pickling/passivation if relevant
VerificationChemistry, tensile or hardness, flattening/flaring/bend, leak/eddy/UT where applicable
CertificationEN 10204 3.1 or other agreed inspection certificate; heat/coil/tube traceability
PackingBlue-wrapped bundles, without pallet/sleeve/slings if requested; moisture protection

Tube manufacturing and acceptance checks

Coil receipt

Record heat number, coil number, coating face/mass, thickness, tensile condition and supplier MTC. A tube made from a compliant coil is not automatically a compliant tube.

Slitting and forming

Confirm strip edge condition, strip width, springback, seam orientation, and coating crack tolerance. High-strength sheet may have limited formability.

Weld process

Identify HF-ERW, TIG or laser; assess weld speed and heat input, seam bead and heat-affected region. High-Cr ferritic tubes need controlled welding and may require post-weld treatment.

Dimensional checks

Measure OD, nominal and minimum wall, out-of-roundness, length, straightness, end squareness and bend/ovality where specified. Use the actual tube standard tolerances.

Nondestructive/leak testing

Apply the specific test prescribed or agreed for the product: eddy-current, ultrasonic, pneumatic or hydrostatic. An inspection technology is not a substitute for the required acceptance level.

Marking and documentation

Record manufacturer, standard, grade, size, batch/heat and inspection results. Any claim to ASTM, EN or GOST should be supported by all relevant mandatory tests.

Example EN purchase descriptions

EN 10346 DX54D+AS120 strip, EN 10143 agreed thickness tolerance, converted into exhaust tubing to drawing [number], OD 76.2 x wall 1.5 x L 5840 mm, specified bend and welded seam performance.

EN 10305-3 E235 + [delivery condition], welded cold-sized precision round tube, OD 101.6 x WT 2.0 x L 5840 mm, dimension class and testing per order.

EN 10296-2 welded stainless mechanical tube in EN 1.4301 (X5CrNi18-10), dimensions and delivery condition per standard and order.

EN 10217-7 welded stainless tube, EN 1.4404, pressure design basis, test category, inspection certificate EN 10204 3.1 and acceptance level as stated.

EU references and verification links

https://www.thyssenkrupp-steel.com/en/products/sheet-coated-products/mild-steel/mild-steel.html

https://www.salzgitter-flachstahl.de/en/products/cold-rolled-products/stahlsorten/mild-steel-grades-for-cold-forming.html

https://ecommerce.sist.si/catalog/standards/cen/65218be8-0680-4489-a0e1-bfba96bb3cfa/en-10346-2026

https://www.ssab.com/en/brands-and-products/steel-categories/coated-steel/metal-coated-formable-steels

https://www.worldstainless.org/files/issf/Education/English/Module_04_What_are_stainless_steels_en.pdf

https://worldstainless.org/wp-content/uploads/2025/12/Ferritic_Stainless_Steels.pdf

https://worldstainless.org/wp-content/uploads/2025/02/Module_05_Corrosion_Resistance_of_Stainless_Steels_en.pdf